According to a rough estimate by biswas 27 for every 100kg limestone charged to the blast furnace the coke rate increases by approximately 2535 kgthm therefore fluxing of the iron ore using prefluxed sinters and pellets and calcination of limestone outside the blast furnace is preferred to avoid extra consumption of coke